PT002 – Planar tension testing:

Load/unload (1 strain or stress level)


Description

A planar tension test is performed at a given crosshead speed. The specimen is loaded to a specified strain or stress level and then unloaded at the same crosshead speed to zero load.  Strain is measured using a non-contact extensometer.

Example Data

               


Temperature Options

This test can generally be performed at any temperature between -80ºC and 250ºC.

  • CT: Cryogenic temperatures (-80ºC to 20ºC)

  • RT: Room temperature (~ 20ºC)

  • HT: High temperatures (20ºC to 250ºC)

Strain Rates

Strain rates up to ~ 1/s are possible, depending on specimen geometry.

Data Provided        

Time, Engineering Strain, Engineering Stress, Load, Crosshead Displacement, Extensometer Measurement

Specimen Requirements        

Specimens must have a width-to-height ratio of 10:1.

Note that we request extra specimens to ensure a sufficient supply of specimens for valid testing.

Veryst can also assist in molding standard and non-standard test specimens.  Please contact us if you are interested in discussing this option.

Replicates Recommended

3